X40MnCrN19/X40MnCrN19K/1.3813 Cold Drawn Steel Bars

Here's what we're working on and thinking about at Vincie.web

Products | Stainless Steels - Special Steels | X40MnCrN19/X40MnCrN19K/1.3813 Cold Drawn Steel Bars

X40MnCrN19/X40MnCrN19K/1.3813 Cold Drawn Steel Bars



X40MnCrN19 X40MnCrN19K 1 3813 Cold Drawn Steel Bars


Delivery Date


Delivery status: Hard-Drawn 、Solutioned 、
Surface: Bright 、
Standard: EN
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other


 
Spec. EN 10308,  EN 10228-2,  EN 10204
The  bars  can  either  be  rolled  or  forged  provided  that the  requested  mechanical  properties  in  cold  drawn condition  are  fulfilled.

Chemical  Composition(Heat analysis  in  weight/%)

c Si Mn P s Cr N
0,30-0,50 <0,50 18,0-20,0 <0,050 <0,015 3,00-5,00 0,080-0,120

Mechanical  Properties
A  hardness  test  shall  be  performed  to  verify  the uniformity  of  the  strength  within  a  delivery  lot  (permelt  and  heat  treatment  batch). 
The  test  amount shall  be  10  %  of  the  bars  with  a  minimum  of  10  bars. When  the  lot  consists  of  less  than  10  bars  all  bars shall  be  tested. 
The  mechanical  properties  are  to  be determined  for  both  the  hardest  and  softest  bar.


0.2%-proof  strength
 
tensile  strength
 
elongation
 
reduction  of  area
 
impact  energy
 
hardness
    10  =5d      
(N/mm2) (N/mm2) (%) (%) (J) HB30
>500 850-1250 >20 >35 S901’ 260  -  360

X40MnCrN19/X40MnCrN19K/1.3813 Cold Drawn Steel Bars Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded